[{"keyword":"\ube14\ub8e8\uc544\uce74","rank":0},{"keyword":"\ubc84\ud29c\ubc84","rank":0},{"keyword":"\uc2a4\ud0c0\ub808\uc77c","rank":0},{"keyword":"\ub9d0\ub538","rank":0},{"keyword":"@","rank":0},{"keyword":"\ub2c8\ucf00","rank":1},{"keyword":"\uadfc\ud29c\ubc84","rank":10},{"keyword":"\uc6d0\uc2e0","rank":2},{"keyword":"\ub9bc\ubc84\uc2a4","rank":-3},{"keyword":"\uc720\ud76c\uc655","rank":-1},{"keyword":"\uac74\ub2f4","rank":4},{"keyword":"\uc778\ubc29","rank":4},{"keyword":"\uc544\ucf54","rank":-5},{"keyword":"\ub77c\uc624","rank":0},{"keyword":"\ud2b8\ub9ad\uceec","rank":-3},{"keyword":"\uc2a4\ud154\ub77c","rank":-5},{"keyword":"\ub358\ud30c","rank":-4},{"keyword":"\uc6d0\ud53c\uc2a4","rank":3},{"keyword":"\ube14\ub8e8","rank":0},{"keyword":"\ud6c4\ubc29","rank":0},{"keyword":"\ub77c\uc778","rank":1},{"keyword":"\uc77c\ubcf8","rank":"new"}]
(IP보기클릭)211.177.***.***
그 글에도 적었지만 신너의 강한 반응성과 휘발성이라는 특성상 약한 신너라고 해서 강한 도료를 못녹이는 것은 아닙니다.
(IP보기클릭)211.177.***.***
그 글에도 적었지만 신너의 강한 반응성과 휘발성이라는 특성상 약한 신너라고 해서 강한 도료를 못녹이는 것은 아닙니다.
(IP보기클릭)223.33.***.***
아하..제가 그부분을 못봤네요. 감사합니다. | 18.12.13 19:58 | |
(IP보기클릭)223.33.***.***
그..반응성과 휘발성 부분에 대해 자세하게 설명해주설수있을까요? 신너라는게 다 다를텐데 왜 반응이 얼어나는건지 이해가 잘안되더군요 | 18.12.13 20:01 | |
(IP보기클릭)223.38.***.***
저도 자세하게는 모르지만 농도차이라고 들었습니다. 락커도료 에나멜도료의 건조시간이 다른것도 그렇다고 합니다. | 18.12.13 20:18 | |
(IP보기클릭)14.34.***.***
답변 감사합니다:) | 18.12.14 10:38 | |
(IP보기클릭)49.169.***.***
(IP보기클릭)14.34.***.***
서로 회사가 달라서 성분이 차이가 나니 그런 것 같습니다. 타미야 아크릴도 알콜계로 알고있는데, 아크릴존만 자주 이러니 당황스럽긴 매한가지입니다만.. | 18.12.14 10:37 | |
(IP보기클릭)223.62.***.***
(IP보기클릭)14.34.***.***
제티팍님 덧글 감사합니다. 회사별 차이가 꽤나 답답하네요... | 18.12.14 10:36 | |
(IP보기클릭)42.82.***.***
(IP보기클릭)14.34.***.***
이게 며칠 방치해뒀다가 이런 문제가 생기는지라..그런데 또 같은 회사 내 아크릴과 에나멜은 또 간섭이 거의 없는 모양이고 마이너 도료쓰면 참 답답하기 그지없네요 ㅠ | 18.12.14 10:39 | |